Causes and characteristics of high self - detonation rate of glass insulator

Oct 01, 2014 Leave a message

1.    Stress stratification of tempered glass

The stress of glass parts is caused by the temperature change during the processing of glass parts.When the glass parts that have been heated to the softening temperature (760~780℃) are cooled quickly, the surface layer shrinks in sudden cooling force, but the internal temperature is still high in the expansion state, resulting in the shrinkage of the surface layer is blocked, leaving compressive stress in the surface layer;Then the internal temperature drops and begins to contract, but at this time the surface layer has hardened, resulting in internal shrinkage obstruction and tensile stress.These two stresses are permanent stresses which are uniformly distributed in the glass pieces until they are completely cooled and the temperature gradient disappears completely.


Once the balance of compressive stress and tensile stress in glass parts of glass insulator is destroyed, cracks will occur rapidly under the action of stress, which will lead to the shattering of glass parts, that is, self-detonation.


2.   Causes and characteristics of self-detonation

       The causes of self-detonation of glass insulators can be divided into two types: the quality of the  product itself and the external operating environment. In practical cases, there are usually two  causes simultaneously.

        (1)Product quality reasons

        (2)External causes

    